Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 5.52 MPa @Temperature 23.0 °C |
801 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ 9570-1 Thermoplastic Elastomer (TPE) Versaflex™ 9570-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Tensile Strength at Break | 5.52 MPa @Temperature 23.0 °C |
801 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ 9570-9 Thermoplastic Elastomer (TPE) Versaflex™ 9570-9 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Tensile Strength at Break | 5.52 MPa @Temperature 23.0 °C |
801 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ CL2250 Thermoplastic Elastomer (TPE) Versaflex™ CL2250 is an easy processing compound designed for use in injection molding applications where FDA compliance, clarity and enhanced heat resistance are required. - Excellent Clarity - Ov.. |
|||
Tensile Strength at Break | 5.52 MPa @Temperature 23.0 °C |
801 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynalloy™ 8900-80 Thermoplastic Elastomer (TPE) Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen.. |
|||
Tensile Strength at Break | 5.52 MPa @Temperature 23.0 °C |
801 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G2706-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2706-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA and medical compliance. - High Puncture Reseal - Overmold Adhesion to Po.. |
|||
Tensile Strength at Break | 5.52 MPa | 801 psi | 510 mm/min; ASTM D412A |
PolyOne Elastamax™ HTE 1101 Styrene Butadiene Block Copolymer (SBC) Information provided by PolyOne |
|||
Tensile Strength at Break | 5.52 MPa | 801 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R158AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |