Tensile Strength at Break 50.6 MPa
7340 psi
UNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
CRP Technology Windform® GF 2.0 Polyamide-Aluminum-Glass Composite
Processed by selective laser sintering (SLS). Windform® GF 2.0 is the evolutionary substitute for Windform GF, our first generation material. Windform® GF 2.0 is a composite material made of poly..