Material Notes:
Processed by selective laser sintering (SLS). Windform® GF 2.0 is the evolutionary substitute for Windform GF, our first generation material. Windform® GF 2.0 is a composite material made of polyamide filled with glass and aluminium, which presents an improvement in both the thermal and mechanical properties, and the aesthetics of the product. In terms of performance, Windform® GF 2.0 shows a significant improvement in the HDT (almost +8%), that is, the heat deflection temperature as well as an increase in the values of tensile strength and elongation strength, therefore offering greater ductility than the previous version,Example Applications: Objects of design and functional aesthetic reproduction, intake manifolds (intake and cooling ducts, air inlet systems), hydraulic ducts (fluid temperature further elevated up to 134°C), fuel systems and household appliances.Information provided by CRP Technology.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.6 MPa
7340 psi
UNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
Elongation at Break 4.6 %
4.6 %
UNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
Tensile Modulus 4.304 GPa
624.3 ksi
UNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
Flexural Strength 80.2 MPa
11600 psi
UNI EN ISO 14125: 2000
Flexural Modulus 3.43 GPa
497 ksi
UNI EN ISO 14125: 2000
Charpy Impact Unnotched 2.185 J/cm²
10.40 ft-lb/in²
ISO 179-1:2007
Charpy Impact, Notched 0.472 J/cm²
2.25 ft-lb/in²
ISO 179-1:2007
Thermal Properties Metric English Comments
Melting Point 179.6 °C
355.3 °F
ISO 11357-2
Deflection Temperature at 1.8 MPa (264 psi) 134.3 °C
273.7 °F
ASTM D648
Vicat Softening Point 168.7 °C
335.7 °F
10 N; ASTM D1252
Electrical Properties Metric English Comments
Volume Resistivity 1e+13 ohm-cm
1e+13 ohm-cm
ASTM D257-93
Surface Resistance 9.1e+13 ohm
9.1e+13 ohm
ASTM D257-93
Descriptive Properties Value Comments
Color Aluminum
Surface Finish 1.8 Ra µm
After Finishing
6.0 Ra µm
After SLS Process