Polymer Property : Tensile Strength at Break = 51.15 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 51.15 MPa
7418 psi
Ambient Cure
Reltek BONDiT™ B-536 Adhesive System
Key Properties: Very high strength bonding of dissimilar materials.High moisture and solvent resistance.Fast ambient cure with good pot life.Ease of use.Applications: Outstanding adhesive for very h..
Tensile Strength at Break 51.15 MPa
7418 psi
Reltek BONDiT™ B-536TH Adhesive System
Key PropertiesVery high strength bonding of dissimilar materials. High moisture and solvent resistance. Fast ambient cure with good pot life. Ease of use. ApplicationsOutstanding adhesive for very h..