Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 36.5 MPa | 5290 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Trilliant™ HC X THC 1100 Natural Copolyester Trilliant™ HC high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Tri.. |
|||
Tensile Strength at Break | 36.5 MPa | 5290 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Edgetek® XT X XT 1000 Natural Copolyester Edgetek™ XT high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Edget.. |
|||
Tensile Strength at Break | 36.5 MPa | 5290 psi | ASTM D638 |
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 27% Plasticizer
(discontinued **) Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro.. |
|||
Tensile Strength at Break | 36.5 MPa | 5290 psi | ASTM D638 |
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 31% Plasticizer
(discontinued **) Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro.. |
|||
Tensile Strength at Break | 36.5 MPa | 5290 psi | 50 mm/min; ISO 527-1,-2 |
Ineos ABS Lustran® M205FC ABS Pellets, Injection Molding Grade Injection Molding grade for medical applications (e.g. inhalers, roller clamps, spikes, etc.)/ Biocompatible with up to 30 days human contact duration according to USP Class VI and ISO 10993-1. Food.. |
|||
Tensile Strength at Break | 36.5 MPa | 5290 psi | ASTM D638 |
IRPC Polimaxx Polene BM3245 PC High Density Polyethylene CHARACTERISTICS:GOOD EXTRUDABILITYHIGH PRESSURE PIPE FOLLOW-UP MINIMUM REQUIRED STRENGTH OF 10.0 MPa (DESIGN STRESS OF 8.0 MPa) CLASSIFICATION PE100BLACK COLOR COMPOUNDAPPLICATIONS:PIPE EXTRUSIONSUI.. |
|||
Tensile Strength at Break | 36.5 MPa | 5290 psi | ASTM D638 |
IRPC Polimaxx Polene GM2860 High Density Polyethylene CHARACTERISTICS: HIGH IMPACT STRENGTH, GOOD PROCESSABILITY, HIGH STIFFNESSAPPLICATIONS: BLOW MOLDING FOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, LUBRICANT BOTTLES COSMETIC BOTTLES, ONE-WAY BOTT.. |
|||
Tensile Strength at Break | 36.5 MPa | 5290 psi | ASTM D638 |
Eastman Tenite 105E3V36327 Acetate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Tensile Strength at Break | 36.5 MPa | 5290 psi | ASTM D638 |
Eastman Tenite 350A0096914 Propionate Natural Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |