Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

IRPC Polimaxx Polene BM3245 PC High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer IRPC Polimaxx
Trade Name Polene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Polene BM3245 PC High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CHARACTERISTICS:GOOD EXTRUDABILITYHIGH PRESSURE PIPE FOLLOW-UP MINIMUM REQUIRED STRENGTH OF 10.0 MPa (DESIGN STRESS OF 8.0 MPa) CLASSIFICATION PE100BLACK COLOR COMPOUNDAPPLICATIONS:PIPE EXTRUSIONSUITABLE FOR WATER SUPPLY PIPE, PRESSURE PIPE, DRAINAGE AND SEWAGE PIPE
Physical Properties Metric English Comments
Density 0.956 g/cc
0.0345 lb/in³
ASTM D792
Environmental Stress Crack Resistance >= 1000 hour
>= 1000 hour
Condition B, F50; ASTM D1693
Carbon Black Loading 2.5 %
2.5 %
ASTM D1603
Melt Flow 0.12 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.12 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
0.55 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.55 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
DIN 53505
Tensile Strength at Break 36.5 MPa
5290 psi
ASTM D638
Tensile Strength, Yield 23.0 MPa
3340 psi
ASTM D638
Elongation at Break 1700 %
1700 %
ASTM D638
Charpy Impact, Notched 1.15 J/cm²
5.47 ft-lb/in²
DIN 53453
Processing Properties Metric English Comments
Processing Temperature 190 - 220 °C
374 - 428 °F
Users viewing this material also viewed the following: