Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 6.62 MPa | 960 psi | 510 mm/min; ASTM D412A |
PolyOne Elastamax™ EG-9090 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9000 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9000 Series of compoun.. |
|||
Tensile Strength at Break | 6.62 MPa | 960 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 121-65M300 Thermoplastic Elastomer
(discontinued **) A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and good.. |
|||
Tensile Strength at Break | 6.62 MPa @Temperature 23.0 °C |
960 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7660-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7660-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Tensile Strength at Break | 6.62 MPa | 960 psi | ASTM D412 |
Teknor Apex Telcar® OBC 4465A Thermoplastic Elastomer Uses: Blow Molding Applications; General Purpose; Soft Touch Applications Forms: Pellets Processing Method: Blow Molding; Profile Extrusion; Sheet Extrusion; Thermoforming; Wire and Cable Extrusion;.. |
|||
Tensile Strength at Break | 6.62 MPa | 960 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 201-64W175 Thermoplastic Elastomer
(discontinued **) A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for thin wall .. |
|||
Tensile Strength at Break | 6.62 MPa | 960 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 221-64W175 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed .. |