Polymer Property : Tensile Strength at Break = 960 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 6.62 MPa
960 psi
510 mm/min; ASTM D412A
PolyOne Elastamax™ EG-9090 Thermoplastic Elastomer (TPE)
The Elastamax™ EG 9000 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9000 Series of compoun..
Tensile Strength at Break 6.62 MPa
960 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 121-65M300 Thermoplastic Elastomer  (discontinued **)
A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and good..
Tensile Strength at Break 6.62 MPa

@Temperature 23.0 °C
960 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7660-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7660-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
Tensile Strength at Break 6.62 MPa
960 psi
ASTM D412
Teknor Apex Telcar® OBC 4465A Thermoplastic Elastomer
Uses: Blow Molding Applications; General Purpose; Soft Touch Applications Forms: Pellets Processing Method: Blow Molding; Profile Extrusion; Sheet Extrusion; Thermoforming; Wire and Cable Extrusion;..
Tensile Strength at Break 6.62 MPa
960 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 201-64W175 Thermoplastic Elastomer  (discontinued **)
A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for thin wall ..
Tensile Strength at Break 6.62 MPa
960 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 221-64W175 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed ..