Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 6.700 MPa | 971.8 psi | Air at 257°F, 168 hr; ASTM D573 |
ExxonMobil Geolast® 701-70 Thermoplastic Elastomer A soft, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applic.. |