Tensile Strength at Break 6.700 MPa
971.8 psi
Air at 257°F, 168 hr; ASTM D573
ExxonMobil Geolast® 701-70 Thermoplastic Elastomer
A soft, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applic..