Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 6.80 MPa | 986 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8221-70 Thermoplastic Elastomer A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Tensile Strength at Break | 6.80 MPa | 986 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8221-75M300 Thermoplastic Elastomer A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and .. |
|||
Tensile Strength at Break | 6.80 MPa | 986 psi | ISO 37 |
Alliance Polymers Viprene™ G65A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G65A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 6.80 MPa | 986 psi | ISO 37 |
Alliance Polymers Viprene™ G65A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G65A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 6.80 MPa | 986 psi | ISO 37 |
Alliance Polymers Viprene™ P60A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 6.80 MPa | 986 psi | ISO 37 |
Alliance Polymers Viprene™ P60A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |