Tensile Strength at Break 6.80 MPa
986 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 8221-70 Thermoplastic Elastomer
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
Tensile Strength at Break 6.80 MPa
986 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 8221-75M300 Thermoplastic Elastomer
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and ..
Tensile Strength at Break 6.80 MPa
986 psi
ISO 37
Alliance Polymers Viprene™ G65A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G65A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Strength at Break 6.80 MPa
986 psi
ISO 37
Alliance Polymers Viprene™ G65A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G65A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Strength at Break 6.80 MPa
986 psi
ISO 37
Alliance Polymers Viprene™ P60A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P60A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Strength at Break 6.80 MPa
986 psi
ISO 37
Alliance Polymers Viprene™ P60A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P60A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..