Mechanical Properties Metric English Comments
Tensile Strength at Break >= 0.414 MPa
>= 60.0 psi
ASTM D412
Parker Chomerics CHO-FORM 5532 EMI Shielding Material
One component, moisture cure, form-in-place EMI gasketing material. This electrically conductive formulation contains silver-plated copper particles dispersed in a silicone elastomer. Cho-Form® 553..
Tensile Strength at Break 0.414 MPa
60.0 psi
ASTM D624
Arlon A3020-B004-12 Silicone Rubber/Fiberglass Laminate  (discontinued **)
Side 1: cured fusible silicone rubber; Substrate: 25% sinusoidal fiberglass; Side 2: cured fusible silicone rubber; Interleave: 1 mil PE film
Tensile Strength at Break 0.414 MPa
60.0 psi
T Block, 1 in<sup>2</sup> (6.45 cm<sup>2</sup>) Jaw Speed 2 in/min (50 mm/min)
3M 4032 Double Coated Urethane Foam Tape
3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst..