Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 479 - 607 MPa | 69500 - 88000 psi | 18-8 Annealed Stainless Steel butt joint. |
Lucas-Milhaupt BRAZE 505 Carbide Brazing Alloy Applications: Braze 505 readily wets nickel and iron base alloys. It is recommended for joining 300 Series stainless steel and will retard interface corrosion in most exposures for which the base m.. |
|||
Tensile Strength at Break | 572 - 607 MPa | 83000 - 88000 psi | Rod, Hot-finished & Solution Annealed |
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar.. |
|||
Tensile Strength at Break | 572 - 607 MPa | 83000 - 88000 psi | Plate, Hot-rolled & Solution Annealed |
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar.. |