Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 572 - 607 MPa | 83000 - 88000 psi | Rod, Hot-finished & Solution Annealed |
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar.. |
|||
Tensile Strength at Break | 572 - 607 MPa | 83000 - 88000 psi | Plate, Hot-rolled & Solution Annealed |
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar.. |