Polymer Property : Tensile Strength at Break = 6090 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 38.0 - 42.0 MPa
5510 - 6090 psi
ASTM D638
Prodways PLASTCure Rigid 10 500 3D Printing Polymer
Superior thermo-mechanical properties.Suitable for the manufacture of parts that require thermal stability, extreme accuracy and quick turnaround. Exceptional for parts that are designed for wind tu..
Tensile Strength at Break 38.0 - 42.0 MPa
5510 - 6090 psi
ASTM D683
Loxim 820 12 HB Polypropylene Compound, Flame Retardant
Information provided by Loxim Industries
Tensile Strength at Break 25.0 - 42.0 MPa
3630 - 6090 psi
TM-019G
AorTech Biomaterials Elast-Eon™ E2-860 Biomedical Polyurethane Pellets
Elast-Eon™ 2-860 is a polyurethane with a 60% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM..
Tensile Strength at Break 25.0 - 42.0 MPa
3630 - 6090 psi
TM-019G
AorTech Biomaterials Elast-Eon™ E2-860 Biomedical Polyurethane Pellets
Elast-Eon™ 2-860 is a polyurethane with a 60% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM..