Mechanical Properties Metric English Comments
Tensile Strength at Break 45.5 MPa
6600 psi
Indium Corp. Indalloy 226 Tin Solder Alloy
Zinc causes high dross U.S. Patent #5,242,658; covers 72.8-89.4Sn 6.7-19.2Zn 2.7-16.4In; temp. range Liq.. 176-193, Sol. 166-191.4Information Provided by Indium Corporation
Tensile Strength at Break 45.5 MPa
6600 psi
machine direction; ASTM D882
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin
DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl..
Tensile Strength at Break 45.5 MPa
6600 psi
ASTM D638
Chase Plastics CP Pryme® N100HSL (COND, 50% RH) Nylon 6, Heat Stabilized, Internally Lubricated
Information provided by Chase Plastics.
Tensile Strength at Break 45.5 MPa
6600 psi
ASTM D638
Chase Plastics CP Pryme® N100L (COND, 50% RH) Nylon 6, Internally Lubricated
Information provided by Chase Plastics.
Tensile Strength at Break 45.5 MPa
6600 psi
machine direction; ASTM D882
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin
DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl..
Tensile Strength at Break 45.5 MPa
6600 psi
machine direction; ASTM D882
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin
DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl..
Tensile Strength at Break 45.5 MPa
6600 psi
machine direction; ASTM D882
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin
DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl..
Tensile Strength at Break 45.5 MPa
6600 psi
machine direction; ASTM D882
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin
DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl..
Tensile Strength at Break 45.5 MPa
6600 psi
90% Ret.
UBE UBESTA® 3030U Nylon 12 (After Hydrochloric Acid (10%) for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Tensile Strength at Break 45.5 MPa
6600 psi
machine direction; ASTM D882
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin
DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl..
Tensile Strength at Break 45.5 MPa
6600 psi
ASTM D638
Chevron Phillips MC3700 High Flow Crystal Polystyrene
DescriptionChevron polystyrene resin MC3700 crystal is a free-flowing, crystal clear polystyrene injection molding compound, designed specifically for thin- and medium-walled or long-flow, difficult..
Tensile Strength at Break 45.5 MPa
6600 psi
ASTM D638
Bayshore Vinyl Compounds BRC R409004/GP.UV Extrusion Compound
BRC R409004/GP.UV is a general purpose medium/high impact profile extrusion compound developed for ease of process, sparkling clarity and gloss. R409004/GP.UV has been formulated for UV resistance ..
Tensile Strength at Break 45.5 MPa
6600 psi
ASTM D638
Bayshore Vinyl Compounds BRC R7550 CLR 223V Extrusion Compound
R7550 CLR 223V is a general purpose medium/high impact profile extrusion compound developed for ease of process, sparkling clarity and gloss. It has been formulated for UV resistance for interior a..