Material Notes:
Zinc causes high dross U.S. Patent #5,242,658; covers 72.8-89.4Sn 6.7-19.2Zn 2.7-16.4In; temp. range Liq.. 176-193, Sol. 166-191.4Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 7.27 g/cc
0.263 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 45.5 MPa
6600 psi
Elongation at Break 85.5 %
85.5 %
Modulus of Elasticity 27.6 GPa
4000 ksi
Thermal Properties Metric English Comments
Melting Point 181 - 187 °C
358 - 369 °F
Solidus 181 °C
358 °F
Liquidus 187 °C
369 °F
Component Elements Properties Metric English Comments
Indium, In 8.8 %
8.8 %
Tin, Sn 83.6 %
83.6 %
Zinc, Zn 7.6 %
7.6 %
Users viewing this material also viewed the following: