Polymer Property : Tensile Strength at Break = 70.0 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 0.483 MPa
70.0 psi
ASTM D624
Arlon A3020-T002-12 Silicone Rubber/Fiberglass Laminate  (discontinued **)
Side 1: cured fusible silicone rubber; Substrate: 25% sinusoidal fiberglass; Side 2: cured fusible silicone rubber; Interleave: 1 mil PE film
Tensile Strength at Break 0.483 MPa
70.0 psi
ASTM D624
Arlon A3020-T004-12 Silicone Rubber/Fiberglass Laminate  (discontinued **)
Side 1: cured fusible silicone rubber; Substrate: 25% sinusoidal fiberglass; Side 2: cured fusible silicone rubber; Interleave: 1 mil PE film