Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon A3020-T002-12 Silicone Rubber/Fiberglass Laminate  (discontinued **)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon A3020-T002-12 Silicone Rubber/Fiberglass Laminate  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Side 1: cured fusible silicone rubber; Substrate: 25% sinusoidal fiberglass; Side 2: cured fusible silicone rubber; Interleave: 1 mil PE film
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
silicone property; Arlon SQA-TMS-024
Thickness 152 microns
6.00 mil
side 1; Arlon SQA-TMS-003
152 microns
6.00 mil
side 2; Arlon SQA-TMS-003
203 microns
8.00 mil
substrate; Arlon SQA-TMS-003
508 microns
20.0 mil
overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
silicone property; ASTM D2240
Tensile Strength at Break 0.483 MPa
70.0 psi
ASTM D624
Tensile Strength, Ultimate 8.27 MPa
1200 psi
silicone property; ASTM D412
Elongation at Break 415 %
415 %
silicone property; ASTM D412
Elongation at Yield 38 %
38 %
ASTM D412
Adhesive Bond Strength 0.0414 MPa
6.00 psi
Arlon SQA-TMS-047
Tear Strength 15.8 kN/m
90.0 pli
Die B; silicone property; ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 24.8 kV/mm
630 kV/in
ASTM D149
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 23.9 °C
12.0 Month

@Temperature 75.0 °F
Descriptive Properties Value Comments
Appearance Translucent