Polymer Property : Tensile Strength at Break = 8.80 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 8.80 MPa
1280 psi
ISO 37
PolyOne OnFlex™ S EF 70A-3S1975 Thermoplastic Elastomer (TPE)
OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell..
Tensile Strength at Break 8.80 MPa
1280 psi
ASTM D412
Sumitomo Chemical ESPOLEX® 4675 Thermoplastic Elastomer
ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi..
Tensile Strength at Break 8.80 MPa
1280 psi
Across Flow; ASTM D412 and ISO 37
ExxonMobil Santoprene® 8211-85M350 Thermoplastic Vulcanizate
Product Description: A hard, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is developed to be used as a skin for molding onto rigid polypropyl..
Tensile Strength at Break 8.80 MPa
1280 psi
Across Flow; ASTM D412 and ISO 37
ExxonMobil Santoprene® 9221-87 Thermoplastic Vulcanizate
Product Description: A hard, colorable UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resista..