ExxonMobil Santoprene® 9221-87 Thermoplastic Vulcanizate

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Exxon Chemical
Trade Name Santoprene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 9221-87 Thermoplastic Vulcanizate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A hard, colorable UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range of applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based, adheres to and is compatible with polypropylene, and is completely recyclable.Key Features:Formulated for good UV resistance and colorfastness.EU and China RoHS compliant.Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D792 and ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 93
93
2 mm; ISO 868
Tensile Strength at Break 8.80 MPa
1280 psi
Across Flow; ASTM D412 and ISO 37
Tensile Stress 5.80 MPa

@Strain 100 %
841 psi

@Strain 100 %
Across Flow; ASTM D412 and ISO 37
Elongation at Break 450 %
450 %
Across Flow; ASTM D412 and ISO 37