Tensile Strength at Break 552 - 586 MPa
80000 - 85000 psi
304 Stainless Steel butt joint
Lucas-Milhaupt BRAZE 380
Characteristics:Braze 380 is a free-flowing, low temperature filler metal with excellent wetting of most ferrous and non-ferrous base metals, and is a good substitute for cadmium-bearing filler meta..
Tensile Strength at Break 552 - 586 MPa
80000 - 85000 psi
304 Stainless Steel butt joint
Lucas-Milhaupt BRAZE 452
Characteristics:Braze 452 is a free-flowing, low temperature filler metal commonly used to replace cadmium-bearing filler metals of similar silver content. This alloy is best suited for narrow gap ..
Tensile Strength at Break 552 - 586 MPa
80000 - 85000 psi
304 Stainless Steel butt joint
Lucas-Milhaupt BRAZE 402 Silver Based Cadmium Free Filler Metal
Characteristics: Braze 402 is a free-flowing, intermediate temperature filler metal and as such is a good substitute for cadmium-bearing filler metals with similar silver contents. The material is ..