Polymer Property : Tensile Strength at Break = 9350 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 64.5 MPa

@Thickness 50.8 mm
9350 psi

@Thickness 2.00 in
ASTM D638
Teknor Apex Synres® PP G20 62 Polypropylene, Glass Reinforced
Notes: The Specialty Compounding Division offers a proprietary line of glass reinforced polypropylene. Typical applications include automotive, building and construction, industrial as well as many ..