Polymer Property : Tensile Strength at Break = 9800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 67.6 MPa
9800 psi
ASTM D638
Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Tensile Strength at Break 67.6 MPa
9800 psi
ASTM D638
Polymer Resources AH-GP1-[color]-H Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength at Break 67.6 MPa
9800 psi
ASTM D638
Polymer Resources AH-GP2 Acetal Homopolymer, Medium Flow, Heat Stabilized
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Tensile Strength at Break 67.6 MPa
9800 psi
ASTM D638
Polymer Resources AH-GP2-[color]-H Acetal Homopolymer, Medium Flow, General Purpose Molding, Heat Stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength at Break 67.6 MPa
9800 psi
ASTM D638
Polymer Resources AH-GP3 Acetal Homopolymer, High Flow Resin, Heat Stabilized
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Tensile Strength at Break 67.6 MPa
9800 psi
ASTM D638
Parker Chomerics PREMIER™ A220-HT EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Tensile Strength at Break 67.6 MPa
9800 psi
ASTM D638
Polymer Resources AH-GP3-[color]-H Acetal Homopolymer, High Flow Resin, Heat Stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength at Break 67.6 MPa
9800 psi
ASTM D638
Polymer Resources AH-GP3 Acetal Homopolymer, High Flow Resin  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength at Break 67.6 MPa
9800 psi
ASTM D 638
Shakespeare Isocorâ„¢ CN30XT Nylon 610
Isocorâ„¢ CN30XT is a low viscosity PA-610 based copolymer. This transparent nylon resin is specifically suited for applications requiring increased solvent resistance and UV stability. Isocor..
Tensile Strength at Break 67.6 MPa
9800 psi
ASTM D638
Techmer ES Electrablend® PPS 06001
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementFeatures: Electrically ConductiveInformation provided by TP Composites, Inc.
Tensile Strength at Break 67.6 MPa

@Temperature 22.8 °C
9800 psi

@Temperature 73.0 °F
ASTM D638
Ensinger TECANYL™ MT Autoclavable Polymer
TECANYL™ MT is a new family of autoclavable materials developed for medical device applications. The material offers the desired performance properties of PPSU based resins with the machining ease..
Tensile Strength at Break 67.6 MPa

@Temperature 22.8 °C
9800 psi

@Temperature 73.0 °F
ASTM D638
Ensinger TECANYL™ MT XRO Autoclavable Polymer
TECANYL™ MT is a new family of autoclavable materials developed for medical device applications. The material offers the desired performance properties of PPSU based resins with the machining ease..
Tensile Strength at Break 67.6 MPa
9800 psi
ASTM D638
Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength  (Unverified Data**)
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength at Break 67.6 MPa
9800 psi
ASTM D638
Polymer Resources AH-GP2 Acetal Homopolymer, Medium Flow, General Purpose Molding  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength at Break 67.6 MPa
9800 psi
ASTM D 638
Shakespeare Isocor™ CN30BT Nylon 610
Isocor™ CN30BT is a medium viscosity PA-610 based copolymer. This transparent nylon resin is specifically suited for applications requiring increased solvent resistance and clarity. Isocor™ CN..