Material Notes:
Isocor™ CN30BT is a medium viscosity PA-610 based copolymer. This transparent nylon resin is specifically suited for applications requiring increased solvent resistance and clarity. Isocor™ CN30BT is also used in applications requiring high modulus and low temperature impact properties. This resin can be processed with conventional techniques. Used for injection molding and film extrusion.Information provided by Shakespeare Company.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D 792
Water Absorption 0.28 %
0.28 %
24 hour immersion; ASTM D 570
Linear Mold Shrinkage 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
Mechanical Properties Metric English Comments
Tensile Strength at Break 67.6 MPa
9800 psi
ASTM D 638
Tensile Modulus 2.30 GPa
333 ksi
ASTM D 638
Izod Impact, Notched 0.587 J/cm
1.10 ft-lb/in
ASTM D 256
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 73.0 °C
163 °F
ASTM D 3418
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified