Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 68.3 MPa | 9900 psi | ASTM D638 |
Parker Chomerics PREMIER™ A220-FR EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Tensile Strength at Break | 68.3 MPa | 9900 psi | ASTM D638 |
Chase Plastics CP Pryme® NN100MD2 (COND, 50% RH) Nylon 66 with 2% MoS2 Lubricated Information provided by Chase Plastics. |
|||
Tensile Strength at Break | 68.3 MPa | 9900 psi | ASTM D638 |
Chase Plastics CP Pryme® PC100RHF Polycarbonate Form: PelletsInformation provided by Chase Plastics. |