Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chase Plastics CP Pryme® NN100MD2 (COND, 50% RH) Nylon 66 with 2% MoS2 Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, MoS2 Filled
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® NN100MD2 (COND, 50% RH) Nylon 66 with 2% MoS2 Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chase Plastics.
Mechanical Properties Metric English Comments
Tensile Strength at Break 68.3 MPa
9900 psi
ASTM D638
Elongation at Break >= 50 %
>= 50 %
ASTM D638
Flexural Strength 71.7 MPa
10400 psi
ASTM D790
Flexural Modulus 1.69 GPa
245 ksi
ASTM D790
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ASTM D256