Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 16.6 MPa @Strain 10.0 % |
2410 psi @Strain 10.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8785 BK482 Polyester Elastomer TPC-ET
(Unverified Data**) Information provided by DuPont Performance Polymers |