Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 215 MPa | 31200 psi | |
Lehmann & Voss LUVOCOM® 1105-7290 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Tensile Stress | 215 MPa | 31200 psi | |
Lehmann & Voss LUVOCOM® 1105-7905 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Tensile Stress | 215 MPa | 31200 psi | |
Lehmann & Voss LUVOCOM® 1105-7909/GY 2 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Chemical and hydrolys.. |
|||
Tensile Stress | 215 MPa | 31200 psi | |
Lehmann & Voss LUVOCOM® TPI-8257 Thermoplastic polyimide, with carbon fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering medical- and electrical enineering, aircraft- and aerospace industry.High-strength and high-stiff parts; lo.. |