Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.52 MPa @Strain 300 % |
511 psi @Strain 300 % |
510 mm/min; ASTM D412A |
PolyOne Elastamax™ XL 0117-5 NATURAL Styrene Butadiene Block Copolymer (SBC) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |