Falling Dart Impact 5.09788 - 5.09788 J

@Temperature -30.0 - -30.0 °C
3.76000 - 3.76000 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 5.10 J Grade Count:1
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and ..
Falling Dart Impact 5.09788 - 5.09788 J

@Thickness 1.78 - 1.78 mm
3.76000 - 3.76000 ft-lb

@Thickness 0.0701 - 0.0701 in
Average value: 5.10 J Grade Count:1
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and ..