Mechanical Properties Metric English Comments
Charpy Impact Unnotched 16.0 J/cm²

@Temperature -20.0 °C
76.1 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVAMID 6 FRM 1 PA6, flame retardant
FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre..
Charpy Impact Unnotched 16.0 J/cm²

@Temperature -20.0 °C
76.1 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVAMID 6 FRM 2 PA6, flame retardant
FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre..
Charpy Impact Unnotched 16.0 J/cm²

@Temperature 23.0 °C
76.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas..
Charpy Impact Unnotched 16.0 J/cm²

@Temperature -30.0 °C
76.1 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® 511DP BK402 Acetal Homopolymer  (Unverified Data**)
Delrin® 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided..
Charpy Impact Unnotched 16.0 J/cm²

@Temperature 23.0 °C
76.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® 511DP BK402 Acetal Homopolymer  (Unverified Data**)
Delrin® 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided..
Charpy Impact Unnotched 16.0 J/cm²

@Temperature -30.0 °C
76.1 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® 911DP BK402 Acetal Homopolymer  (Unverified Data**)
Delrin® 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided by..
Charpy Impact Unnotched 16.0 J/cm²

@Temperature 23.0 °C
76.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® 911DP BK402 Acetal Homopolymer  (Unverified Data**)
Delrin® 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided by..
Charpy Impact Unnotched 16.0 J/cm²

@Temperature 23.0 °C
76.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG500AL is a medium viscosity acetal homopolymer, lubricated for low wear and /or coefficient of friction. It has been developed for consideration into applications such as parts for the fo..
Charpy Impact Unnotched 16.0 J/cm²

@Temperature -30.0 °C
76.1 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG500TL medium viscosity acetal homopolymer resin containing 1.5% Teflon® PTFE Micropowder. It has been developed for consideration into applications such as parts for the food industry.In..
Charpy Impact Unnotched 16.0 J/cm²

@Temperature -30.0 °C
76.1 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Lanxess Pocan® S 7926 000000 PBT
PBT, non-reinforced, injection molding, extrusion, flame retardant, impact modified
Charpy Impact Unnotched 16.0 J/cm²

@Temperature 23.0 °C
76.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1eU
Lanxess Durethan® A 30 H3.0 000000 Nylon 66
PA 66, non reinforced, injection molding, heat-ageing stabilized
Charpy Impact Unnotched 16.0 J/cm²

@Temperature 23.0 °C
76.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Styrolution Luran® S KR 2859 ASA
Description: Stiff extrusions product, versatile grade for profile and sheet extrusion as protective cap layer.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Charpy Impact Unnotched 16.0 J/cm²

@Temperature 23.0 °C
76.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Styrolution Luran® S KR 2859 UV ASA
Description: Stiff extrusions product, versatile grade for profile and sheet extrusion as protective cap layer.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Charpy Impact Unnotched <= 16.0 J/cm²

@Temperature -30.0 °C
<= 76.1 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Styrolution Polystyrol 486 M GR 2 PS
Description: Polystyrol 486 M is a normal flowing, high-impact grade that is especially suitable for blends with a high proportion of general-purpose Polystyrol (preferably Polystyrol 165 H or Polys..
Charpy Impact Unnotched 16.0 J/cm²

@Temperature -30.0 °C
76.1 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Styrolution Terluran® HI-12 ABS
Terluran HI-12 is an injection molding grade of ABS with a very high toughness and easy flow.Very high toughnessEasy flowingUL 94 HB (1.6 & 3.2 mm)Information provided by Styrolution
Charpy Impact Unnotched 16.0 J/cm²

@Temperature -30.0 °C
76.1 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Styrolution Novodur® H801 ABS / PC
Novodur H801 is a high heat injection molding grade with high impact strength and reduced emission.Information provided by Styrolution
Charpy Impact Unnotched 16.0 J/cm²

@Temperature 23.0 °C
76.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
BASF Ultraform® W2320 U03 POM
Description: Very free-flowing, rapidly solidifying grade with UV stabilization for use where processing is extremely difficult but mechanical requirements are lower.Information provided by BASF
Charpy Impact Unnotched 16.0 J/cm²

@Temperature -30.0 °C
76.1 ft-lb/in²

@Temperature -22.0 °F
DIN ISO 179
BASF Elastollan R 1001 10% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
Charpy Impact Unnotched 16.0 J/cm²

@Temperature 23.0 °C
76.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® 911DP NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided by..