Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 16.0 J/cm² @Temperature -20.0 °C |
76.1 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 FRM 1 PA6, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre.. |
|||
Charpy Impact Unnotched | 16.0 J/cm² @Temperature -20.0 °C |
76.1 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 FRM 2 PA6, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre.. |
|||
Charpy Impact Unnotched | 16.0 J/cm² @Temperature 23.0 °C |
76.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas.. |
|||
Charpy Impact Unnotched | 16.0 J/cm² @Temperature -30.0 °C |
76.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 511DP BK402 Acetal Homopolymer
(Unverified Data**) Delrin® 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided.. |
|||
Charpy Impact Unnotched | 16.0 J/cm² @Temperature 23.0 °C |
76.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 511DP BK402 Acetal Homopolymer
(Unverified Data**) Delrin® 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided.. |
|||
Charpy Impact Unnotched | 16.0 J/cm² @Temperature -30.0 °C |
76.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 911DP BK402 Acetal Homopolymer
(Unverified Data**) Delrin® 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided by.. |
|||
Charpy Impact Unnotched | 16.0 J/cm² @Temperature 23.0 °C |
76.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 911DP BK402 Acetal Homopolymer
(Unverified Data**) Delrin® 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided by.. |
|||
Charpy Impact Unnotched | 16.0 J/cm² @Temperature 23.0 °C |
76.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500AL is a medium viscosity acetal homopolymer, lubricated for low wear and /or coefficient of friction. It has been developed for consideration into applications such as parts for the fo.. |
|||
Charpy Impact Unnotched | 16.0 J/cm² @Temperature -30.0 °C |
76.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500TL medium viscosity acetal homopolymer resin containing 1.5% Teflon® PTFE Micropowder. It has been developed for consideration into applications such as parts for the food industry.In.. |
|||
Charpy Impact Unnotched | 16.0 J/cm² @Temperature -30.0 °C |
76.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Pocan® S 7926 000000 PBT PBT, non-reinforced, injection molding, extrusion, flame retardant, impact modified |
|||
Charpy Impact Unnotched | 16.0 J/cm² @Temperature 23.0 °C |
76.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Lanxess Durethan® A 30 H3.0 000000 Nylon 66 PA 66, non reinforced, injection molding, heat-ageing stabilized |
|||
Charpy Impact Unnotched | 16.0 J/cm² @Temperature 23.0 °C |
76.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Styrolution Luran® S KR 2859 ASA Description: Stiff extrusions product, versatile grade for profile and sheet extrusion as protective cap layer.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact Unnotched | 16.0 J/cm² @Temperature 23.0 °C |
76.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Styrolution Luran® S KR 2859 UV ASA Description: Stiff extrusions product, versatile grade for profile and sheet extrusion as protective cap layer.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact Unnotched | <= 16.0 J/cm² @Temperature -30.0 °C |
<= 76.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Styrolution Polystyrol 486 M GR 2 PS Description: Polystyrol 486 M is a normal flowing, high-impact grade that is especially suitable for blends with a high proportion of general-purpose Polystyrol (preferably Polystyrol 165 H or Polys.. |
|||
Charpy Impact Unnotched | 16.0 J/cm² @Temperature -30.0 °C |
76.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution Terluran® HI-12 ABS Terluran HI-12 is an injection molding grade of ABS with a very high toughness and easy flow.Very high toughnessEasy flowingUL 94 HB (1.6 & 3.2 mm)Information provided by Styrolution |
|||
Charpy Impact Unnotched | 16.0 J/cm² @Temperature -30.0 °C |
76.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution Novodur® H801 ABS / PC Novodur H801 is a high heat injection molding grade with high impact strength and reduced emission.Information provided by Styrolution |
|||
Charpy Impact Unnotched | 16.0 J/cm² @Temperature 23.0 °C |
76.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultraform® W2320 U03 POM Description: Very free-flowing, rapidly solidifying grade with UV stabilization for use where processing is extremely difficult but mechanical requirements are lower.Information provided by BASF |
|||
Charpy Impact Unnotched | 16.0 J/cm² @Temperature -30.0 °C |
76.1 ft-lb/in² @Temperature -22.0 °F |
DIN ISO 179 |
BASF Elastollan R 1001 10% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Charpy Impact Unnotched | 16.0 J/cm² @Temperature 23.0 °C |
76.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 911DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided by.. |