Mechanical Properties Metric English Comments
Charpy Impact Unnotched 25.0 J/cm²

@Temperature 23.0 °C
119 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® 100AL NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 100AL NC010 an unreinforced, high viscosity, lubricated acetal homopolymer resin, containing an advanced system of lubrication for low wear and friction against metals and plastics.Informat..
Charpy Impact Unnotched 25.0 J/cm²

@Temperature 23.0 °C
119 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Styrolution Luran® S 777 K UV Black 56625 ASA
Description: Easy flowing injection molding grade with good toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Charpy Impact Unnotched 25.0 J/cm²

@Temperature 23.0 °C
119 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Styrolution Luran® S 778 Q42 Colored ASA
Description: Injection molding grade with enhanced toughness and resistance to heat distortion. Especially suitable for exterior automotive components (e.g. radiator grills, rear end appliqué pan..
Charpy Impact Unnotched 25.0 J/cm²

@Temperature 23.0 °C
119 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Styrolution Luran® S 778 TE Black 25991 ASA
Description: Extrusion grade with enhanced toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Charpy Impact Unnotched 25.0 J/cm²

@Temperature 23.0 °C
119 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Styrolution Luran® S 778 TE UV Colored ASA
Description: Extrusion grade with enhanced toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Charpy Impact Unnotched 25.0 J/cm²

@Temperature 23.0 °C
119 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Styrolution Luran® S 778 UV Colored ASA
Description: Injection molding grade with enhanced toughness and resistance to heat distortion. Especially suitable for exterior automotive components (e.g. radiator grills, rear end appliqué pan..
Charpy Impact Unnotched 25.0 J/cm²

@Temperature 23.0 °C
119 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Styrolution Luran® S 796 M Colored ASA
Description: High-impact injection molding gr4ade with good flowability.Applications: Trim panels for goods vehicles.Information provided by STYROLUTION, which is a joint venture between BASF and IN..
Charpy Impact Unnotched 25.0 J/cm²

@Temperature 23.0 °C
119 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Styrolution Luran® S 797 S UV White 33999 Q455 ASA
Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN..
Charpy Impact Unnotched 25.0 J/cm²

@Temperature 23.0 °C
119 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Styrolution Luran® S 797 S White 35962 ASA
Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN..
Charpy Impact Unnotched 25.0 J/cm²

@Temperature 23.0 °C
119 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
BASF Ultraform® H2320 004 POM
Description: Is a POM, high-molecular-weight grade for extrusion of small thin-walled pipes and panel.Information provided by BASF
Charpy Impact Unnotched 25.0 J/cm²

@Temperature 23.0 °C
119 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
BASF Ultraform® N2320 U035 POM
Description: Is a POM, UV-stabilized injection-molding grade.Information provided by BASF
Charpy Impact Unnotched 25.0 J/cm²

@Temperature 23.0 °C
119 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
BASF Ultraform® S2320 0035 LEV POM
Description: Is a POM, free-flowing and rapidly solidifying standard grade with reduced emission potential for injection molding.Information provided by BASF
Charpy Impact Unnotched 25.0 J/cm²

@Temperature 23.0 °C
119 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
BASF Ultraform® S2320 0035 POM
Description: Is a POM, free-flowing and rapidly solidifying standard grade with improved impact strength for injection molding.Information provided by BASF
Charpy Impact Unnotched 25.0 J/cm²

@Temperature -30.0 °C
119 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® 311DP NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It has improved dimensional stability, high strengt..
Charpy Impact Unnotched 25.0 J/cm²

@Temperature -30.0 °C
119 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG311DP is a medium-high viscosity acetal homopolymer, with improved thermal stability and modifications for more precise molding. It has been developed for consideration into applications ..
Charpy Impact Unnotched 25.0 J/cm²

@Temperature 23.0 °C
119 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® FG100AL NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG100AL is a high viscosity, lubricated acetal homopolymer resin, containing an advanced system of lubrication. It has been developed for consideration into applications such as parts for t..
Copyright © lookpolymers.com All Rights Reserved