Mechanical Properties Metric English Comments
Charpy Impact Unnotched 5.40 J/cm²

@Temperature -20.0 °C
25.7 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Polykemi AB POLYfill PP CQX15015 R3 UV Polypropylene, Mineral Reinforced, Scratch Resistant
Information provided by Polykemi AB
Charpy Impact Unnotched 5.40 J/cm²

@Temperature -30.0 °C
25.7 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® S RV150 (cond.) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Charpy Impact Unnotched 5.40 J/cm²

@Temperature -30.0 °C
25.7 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 179/1eU
DuPont Performance Polymers Zytel® 79G13HSL BK039 Nylon 66  (Unverified Data**)
Zytel® 79G13HSL BK039 is a 13 % glass reinforced, heat stabilized, lubricated slightly toughened black polyamide 66 for injection molding. It has improved impact resistance.Information provided by ..
Charpy Impact Unnotched 5.40 J/cm²

@Temperature -30.0 °C
25.7 ft-lb/in²

@Temperature -22.0 °F
ISO 179
LG Chemical AF-320T ABS, Flame Retardant, High Impact, High Flow, Slim Wall
Information Provided by LG Chem
Charpy Impact Unnotched 5.40 J/cm²

@Temperature 23.0 °C
25.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Sax Polymers SAXAMID 126F4 Nylon 6, 20% Glass Fiber
SAXAMID 126F4 is a polyamide 6 injection-molding-grade reinforced with 20% glass fibers.Information provided by SAX Polymers
Charpy Impact Unnotched 5.40 J/cm²

@Temperature 23.0 °C
25.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Sax Polymers SAXAMID 226F6RY01 Nylon 6.6, 30% Glass Fiber
SAXAMID 226F6RY01 is a polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers
Charpy Impact Unnotched 5.40 J/cm²

@Temperature -20.0 °C
25.7 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eU
Borealis Xmod™ GD301FE Polypropylene, Glass Fiber Reinforced
Xmod™ GD301FE is a 30 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also a..
Charpy Impact Unnotched 5.40 J/cm²

@Temperature 23.0 °C
25.7 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eU
DSM Novamid® 1010GN2-30 NAT/BK37 PA6-GF30 FR(17)
30% Glass Reinforced, Flame Retardant
Charpy Impact Unnotched 5.40 J/cm²

@Temperature 23.0 °C
25.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® FG570 NC000 Acetal Homopolymer
Delrin® FG570 NC000 is a medium viscosity acetal homopolymer containing 20% glass fiber for injection molding. It has high stiffness and low warpage. It has been developed for consideration in appl..
Charpy Impact Unnotched 5.40 J/cm²

@Temperature -30.0 °C
25.7 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 179/1eU
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66  (Unverified Data**)
Zytel® 79G13HSL is a 13% glass fiber reinforced, heat stabilized, lubricated slightly toughened polyamide 66 for injection molding. It has improved impact resistance.Information provided by DuPont ..
Charpy Impact Unnotched 5.40 J/cm²

@Temperature -20.0 °C
25.7 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eU
Borealis Xmod™ GB306SAF Polypropylene, Glass Fiber Reinforced
Xmod™ GB306SAF is a 35 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. The product is available in standard black 9502. This mat..
Charpy Impact Unnotched 5.40 J/cm²

@Temperature -30.0 °C
25.7 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultradur® B 4300 G4 FC 20% Glass Filled PBT
Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation..