Material Notes:
Xmod™ GD301FE is a 30 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. The product is available in standard black 9502. Applications: front end carriers, door module carriers, fans and shrouds, pump housings, pedal carriers, and air bag housings.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0095 cm/cm
0.0095 in/in
Borealis Method
Melt Flow 4.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 106 MPa
15400 psi
ISO 527-2
Elongation at Break 3.2 %
3.2 %
50mm/min; ISO 527-2
Tensile Modulus 7.50 GPa
1090 ksi
1mm/min; ISO 527-2
Flexural Strength 145 MPa
21000 psi
ISO 178
Flexural Modulus 6.50 GPa
943 ksi
2mm/min; ISO 178
Charpy Impact Unnotched 5.40 J/cm²

@Temperature -20.0 °C
25.7 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eU
5.90 J/cm²

@Temperature 23.0 °C
28.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 148 °C
298 °F
ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 158 °C
316 °F
ISO 75-2
Vicat Softening Point 139 °C

@Load 5.10 kg
282 °F

@Load 11.2 lb
ISO 306
Processing Properties Metric English Comments
Processing Temperature 230 - 280 °C
446 - 536 °F
mass temperature
Feed Temperature 40.0 - 80.0 °C
104 - 176 °F
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Injection Velocity 1667 - 3333 mm/sec
65.63 - 131.2 in/sec
Hold Pressure 3.00 - 6.00 MPa
435 - 870 psi
Descriptive Properties Value Comments
Back Pressure as low as possible
Emission (µgC/g) < 50
VDA 277
Fogging (mg) < 2
DIN 75201
Screw Speed low to medium