Polymer Property : Charpy Impact Unnotched = 3.20 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 3.20 J/cm²

@Temperature 23.0 °C
15.2 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Plastcom PLASTALEN® PH 52 T 20 003/1M Polypropylene reinforced with 20% mineral filler
PP homopolymer for injection molding with the content of 20 % mineral filler, heat stabilized. Application in automotive industry. Delivered in black grade.Information Provided by Plastcom spol. s r..
Charpy Impact Unnotched 3.20 J/cm²

@Temperature -20.0 °C
15.2 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN EQ 18 N PP, basic type
FeaturesModified PE with special heat and processional stabilization. Application in extrusion of profiles and pipes, blowing of bottles and jerrycans. Delivered in black colour.Packaging, transport..
Charpy Impact Unnotched 3.20 J/cm²

@Temperature 23.0 °C
15.2 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Plastcom SLOVALEN PH 51 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc
FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 130°C...
Charpy Impact Unnotched 3.20 J/cm²

@Temperature -20.0 °C
15.2 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN PH 91 N PP, basic type
FeaturesCompounded homopolymer PP. General use in all industry branches. Packing material, garden flower-pots, toys, furniture industry, guides, dowels, clamps, office chairs, holders etc. Delivered..
Charpy Impact Unnotched 3.20 J/cm²

@Temperature -20.0 °C
15.2 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVAMID 66 GB 30 LS PA66, 30% glass beads, light stability
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
Charpy Impact Unnotched 3.20 J/cm²

@Temperature -20.0 °C
15.2 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVAMID 66 GF 15 GB 25 TS PA66, 15% glass fibre, 25% glass beads
FeaturesPA 66 chemically reinforced with 15 % glass fibre and with the content of 25% glass beads, thermo stable. Improved anisotropy of shrinkage. The relation of the anisotropy to the mechanical p..
Charpy Impact Unnotched 3.20 J/cm²

@Temperature 23.0 °C
15.2 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVAMID 66 T 40 FRO 3 PA66, 40% mineral filling, flame retardant
FeaturesPA 66 with the content of 40% chemically modified mineral filling a with fire retardant. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat produ..
Charpy Impact Unnotched 3.20 J/cm²

@Temperature 23.0 °C
15.2 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Plastcom SLOVAMID 66 T 40 Polyamide 66, 40% Mineral Filled
FeaturesPA 66 with the content of 40% chemically modified mineral filling. Used for holders of electric hand tools, hobby tools, gears, covers of electric tools, flat products, automobile wheel cov..
Charpy Impact Unnotched 3.20 J/cm²

@Temperature -30.0 °C
15.2 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Polykemi AB SCANBLEND P AP2060 F20 PBT/ASA, Glass Fiber Reinforced
Information provided by Polykemi AB
Charpy Impact Unnotched 3.20 J/cm²

@Temperature -30.0 °C
15.2 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® A RV150 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact Unnotched 3.20 J/cm²

@Temperature 23.0 °C
15.2 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Plastcom PLASTALEN® PH 52 T 20 Polypropylene reinforced with mineral filler
PP homopolymer for injection molding with the content of 20 % mineral filler, heat stabilized. Application in automotive industry. Delivered in black grade.Information Provided by Plastcom spol. s r..
Charpy Impact Unnotched 3.20 J/cm²

@Temperature 23.0 °C
15.2 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DuPont Performance Polymers Rynite® FR515 BK507 PET  (Unverified Data**)
Rynite® FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm(0.03in). Has a 140C temp index. Excellent balance of electr..
Charpy Impact Unnotched 3.20 J/cm²

@Temperature -30.0 °C
15.2 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM
Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features..
Charpy Impact Unnotched 3.20 J/cm²

@Temperature -30.0 °C
15.2 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM
Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica..
Charpy Impact Unnotched 3.20 J/cm²

@Temperature -20.0 °C
15.2 ft-lb/in²

@Temperature -4.00 °F
LATI Latilon 28D G/30 PC, 30% Glass Fiber Reinforced
Polycarbonate (PC) based compound. Glass fibers. Low smoke density and low toxicity index. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A..