Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 6.60 J/cm² @Temperature -30.0 °C |
31.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, Conditioned Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Charpy Impact Unnotched | 6.60 J/cm² @Temperature -30.0 °C |
31.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, Conditioned Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Charpy Impact Unnotched | 6.60 J/cm² @Temperature -30.0 °C |
31.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, Conditioned Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
Charpy Impact Unnotched | 6.60 J/cm² @Temperature -30.0 °C |
31.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, Conditioned Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
Charpy Impact Unnotched | 6.60 J/cm² @Temperature -30.0 °C |
31.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Ascend Performance Materials Vydyne® R525 Nylon 66, 25% Glass Reinforced, Conditioned Vydyne® R525 is hydrolysis-resistant, 25% glass-fiber reinforced PA66 resin. Available in natural it is lubricated for improved machine feed and flow. Glass-reinforced Vydyne resins provide higher .. |
|||
Charpy Impact Unnotched | 6.60 J/cm² @Temperature -30.0 °C |
31.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Conditioned (2.5% Moisture) Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe.. |