Polymer Property : Charpy Impact Unnotched = 6.60 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 6.60 J/cm²

@Temperature -30.0 °C
31.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, Conditioned
Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
Charpy Impact Unnotched 6.60 J/cm²

@Temperature -30.0 °C
31.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, Conditioned
Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
Charpy Impact Unnotched 6.60 J/cm²

@Temperature -30.0 °C
31.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, Conditioned
Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
Charpy Impact Unnotched 6.60 J/cm²

@Temperature -30.0 °C
31.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, Conditioned
Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
Charpy Impact Unnotched 6.60 J/cm²

@Temperature -30.0 °C
31.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Ascend Performance Materials Vydyne® R525 Nylon 66, 25% Glass Reinforced, Conditioned
Vydyne® R525 is hydrolysis-resistant, 25% glass-fiber reinforced PA66 resin. Available in natural it is lubricated for improved machine feed and flow. Glass-reinforced Vydyne resins provide higher ..
Charpy Impact Unnotched 6.60 J/cm²

@Temperature -30.0 °C
31.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Conditioned (2.5% Moisture)
Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe..