Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® K-FHG12 (Dry) 60% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® K-FHG12 (Cond.) 60% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® K224-G8U (Cond.) 43% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® K224-HG8 (Cond.) 40% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® K224-HG8 Nylon 6-40% Glass Reinforced (European Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® Ultraflow™ K-FG0 Nylon 6-50% Glass Reinforced (European and Asian Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® Ultraflow™ K-FG0 Nylon 6-50% Glass Reinforced (European and Asian Grade) (Dry)
(discontinued **)& The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® Ultraflow™ K-FG12 Nylon 6-60% Glass Reinforced (European Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® Ultraflow™ K-FG12 Nylon 6-60% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® K224-G0 Nylon 6-50% Glass Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® K224-G0 Nylon 6-50% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® K224-HG7 (Cond.) 35% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® K224-HG7 Nylon 6-35% Glass Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K224-LG6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® K224-PG8 (Cond.) 40% Glass Reinforced, Impact Modified Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® K224-PG8 Impact Modified Nylon 6-40% Glass Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® Ultraflow™ K-FHG0 Nylon 6-50% Glass Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® Ultraflow™ K-FHG12 Nylon 6-60% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Stanyl® TW200F8 Nylon 46-40% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Stanyl® TW241F8 Nylon 46-40% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/eU |
Eurotec® Tecomid® NA40 GR50 NL PA 6.6 50% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/eU |
Eurotec® Tecomid® NB40 GR40 NL PA 6 40% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® K224-G0 (Dry) 50% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® Ultraflow™ K-FHG0 Nylon 6-50% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Conditioned Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Ascend Performance Materials VYDYNE® R533H Nylon, 33% Glass Reinforced, Conditioned Vydyne® R533H is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when exposed to anti-free.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R533T Nylon 66, Translucent, 33% Glass Filled, Conditioned (2.5% Moisture) The Vydyne® R533T is a translucent 33% glass reinforced heat stabilized Nylon 66 product specifically designed for use in power steering reservoirs and other applications where chemical resistance,.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® K-FHG0 (Cond.) 50% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |