Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurotec® Tecomid® NB40 GR40 NL PA 6 40% glass fiber reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Eurotec
Trade Name Tecomid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurotec® Tecomid® NB40 GR40 NL PA 6 40% glass fiber reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good chemical resistanceGood flow and processing propertiesAPPLICATIONS: AutomotiveElectrical/ElectronicFurnitureConstructionHome appliances
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
ISO 1183
Filler Content 40 %
40 %
ISO 3451
Moisture Absorption at Equilibrium 1.8 %
1.8 %
Humidity Absorption, 50% RH, 23°C; ISO 62
Water Absorption at Saturation 5.5 %
5.5 %
23°C; ISO 62
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 195 MPa
28300 psi
ISO 527
Elongation at Break 3.0 %
3.0 %
ISO 527
Tensile Modulus 12.0 GPa
1740 ksi
ISO 527
Flexural Strength 270 MPa
39200 psi
ISO 178
Flexural Modulus 9.50 GPa
1380 ksi
ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²

@Temperature -30.0 °C
7.14 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
19.0 kJ/m²

@Temperature 23.0 °C
9.04 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched 8.50 J/cm²

@Temperature -30.0 °C
40.5 ft-lb/in²

@Temperature -22.0 °F
ISO 179/eU
10.0 J/cm²

@Temperature 23.0 °C
47.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/eU
Charpy Impact, Notched 1.60 J/cm²

@Temperature -30.0 °C
7.61 ft-lb/in²

@Temperature -22.0 °F
ISO 179/eA
2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
ISO 179/eA
Thermal Properties Metric English Comments
Melting Point 223 °C
433 °F
10 K/min; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75-1/2
Deflection Temperature at 1.8 MPa (264 psi) 212 °C
414 °F
ISO 75-1/2
Vicat Softening Point 215 °C
419 °F
50N; ISO 306
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Glow Wire Test 650 °C

@Thickness 2.00 mm
1200 °F

@Thickness 0.0787 in
plaque; IEC 60695
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Comparative Tracking Index 500 V
500 V
IEC 60112
Users viewing this material also viewed the following: