Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.00 - 1.20 J/cm² @Temperature 23.0 °C |
4.76 - 5.71 ft-lb/in² @Temperature 73.4 °F |
Compression; ISO 179/ 1eU |
Raschig Group AMPLA® 7500 melamine-modified polyester Organically and inorganically filled melamine modified Polyester molding compound. Low post-shrinkage, very good electrical values, excellent heat resistance, very good sliding behavior and wear sta.. |
|||
Charpy Impact Unnotched | 0.700 - 1.20 J/cm² @Temperature 23.0 °C |
3.33 - 5.71 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eU |
Raschig Group MELOPLAS® 152 MF Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al.. |
|||
Charpy Impact Unnotched | 0.700 - 1.20 J/cm² @Temperature 23.0 °C |
3.33 - 5.71 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eU |
Raschig Group MELOPLAS® 181.5 MF Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. Very good electrical properties, high surface hardness, good mechanical strength, high UV and heat resis.. |