Polymer Property : Charpy Impact Unnotched = 59.5 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 12.5 J/cm²

@Temperature 23.0 °C
59.5 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Lanxess Durethan® DP 1802 H3.0 000000 Nylon 6
PA 6 injection and extrusion molding grade, non-reinforced, impact-modified, UL 94V-2 off 0,75 mm, GWIT: 775°C off 0,75 mm, halogen-free
Charpy Impact Unnotched 12.5 J/cm²

@Temperature 23.0 °C
59.5 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Styrolution Terluran® GP-25 ABS
Terluran GP-25 is an easy-flow, general purpose injection molding grade with high resistance to impact and heat distortion; intended for a wide range of applications, particularly in the housings se..
Charpy Impact Unnotched 12.5 J/cm²

@Temperature 23.0 °C
59.5 ft-lb/in²

@Temperature 73.4 °F
ISO 179/eU
Eurotec® Tecomid® NA40 MR15 NL IL PA 6.6 15% mineral reinforced, impact modified
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Charpy Impact Unnotched 12.5 J/cm²

@Temperature -30.0 °C
59.5 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DSM Stanyl® TE350 Nylon 46 (European and Asian Grade) (Cond)  (discontinued **)
Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie..