Charpy Impact Unnotched 6.80 J/cm²

@Temperature 23.0 °C
32.4 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVAMID 6 GF 30 FRG 4 LW PA6, 30% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fibre, with nonhalogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°..
Charpy Impact Unnotched 6.80 J/cm²

@Temperature 23.0 °C
32.4 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVAMID 6 GF 30 FRGG2 PA6, 30% glass fibre, flame retardant
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
Charpy Impact Unnotched 6.80 J/cm²

@Temperature 23.0 °C
32.4 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Plastcom SLOVAMID® 6 GF 30 FRG 2 PA6 reinforced with glass fiber, flame retarded
PA 6 for injection molding, reinforced with 30 % glass fiber, flame retarded with halogen free flame retardant. Main features: flammability in accordance with UL 94 5 at 3.2 mm. Application for the ..
Charpy Impact Unnotched 6.80 J/cm²

@Temperature 23.0 °C
32.4 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® A ERV3012 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact Unnotched 6.80 J/cm²

@Temperature -30.0 °C
32.4 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® S CP300 (cond.) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Charpy Impact Unnotched 6.80 J/cm²

@Temperature -20.0 °C
32.4 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN PC 93 T 15 1/M PP, 15% mineral filling, UV stability
FeaturesModified PP for injection moulding with the content of 15 % mineral filling, uv stabilized. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased..
Charpy Impact Unnotched 6.80 J/cm²

@Temperature -30.0 °C
32.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Sax Polymers SAXAMID 126F5 Nylon 6, 25% Glass Fiber
SAXAMID 126F5 is a polyamide 6 injection-molding-grade reinforced with 25% glass fibers.Information provided by SAX Polymers
Charpy Impact Unnotched 6.80 J/cm²

@Temperature 23.0 °C
32.4 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eU
DSM Novamid® 3010GN30 NAT PA66-GF30 FR(17)
30% Glass Reinforced, Flame Retardant
Charpy Impact Unnotched 6.80 J/cm²

@Temperature -30.0 °C
32.4 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eU
DuPont Performance Polymers Zytel® PLUS PLS95G35DH1 BK031 Nylon
Zytel® PLS95G35DH1 BK031is a high flow 35% glass reinforced PA using SHIELD Technology, only from DuPont, combining excellent surface appearance, excellent welding and fatigue retention, exceptiona..
Charpy Impact Unnotched 6.80 J/cm²

@Temperature -30.0 °C
32.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Ascend Performance Materials Vydyne® R535H NT651 Nylon 66, 35% Glass Reinforced, DAM
Vydyne® R535H NT651 is 35% glass-fiber reinforced PA66 resin. Available in natural, it is heat-stabilized with an electrically neutral heat stabilizer. It is designed specially for electrical appli..