Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 8.27 MPa @Temperature 150 °C |
1200 psi @Temperature 302 °F |
Lap Shear Strength vs. Aluminum |
Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Adhesive Bond Strength | 8.30 MPa @Temperature 25.0 °C |
1200 psi @Temperature 77.0 °F |
tube shears |
Henkel Hysol MA 562 Core Splice Adhesive General-purpose 250°F / 121°C or 350°F / 177°C curing foaming adhesive. Designed for service temperatures from -67°F / -55°C to 350°F / 177°C. Medium tack, nonmetallic, low exotherm properti.. |