Polymer Property : Adhesive Bond Strength = 1410 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 9.70 MPa

@Temperature 23.9 °C
1410 psi

@Temperature 75.0 °F
on steel; ASTM D1002-64
3M Pronto™ CA-40 Instant Adhesive
One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.Very fast setting adhesive with..
Adhesive Bond Strength 9.70 MPa

@Temperature 23.9 °C
1410 psi

@Temperature 75.0 °F
on aluminum; ASTM D1002-64
3M Pronto™ CA-40 Instant Adhesive
One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.Very fast setting adhesive with..