Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 9.70 MPa @Temperature 23.9 °C |
1410 psi @Temperature 75.0 °F |
on steel; ASTM D1002-64 |
3M Pronto™ CA-40 Instant Adhesive One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.Very fast setting adhesive with.. |
|||
Adhesive Bond Strength | 9.70 MPa @Temperature 23.9 °C |
1410 psi @Temperature 75.0 °F |
on aluminum; ASTM D1002-64 |
3M Pronto™ CA-40 Instant Adhesive One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.Very fast setting adhesive with.. |