Mechanical Properties Metric English Comments
Adhesive Bond Strength 15.0 MPa

@Thickness 0.750 mm
2180 psi

@Thickness 0.0295 in
Lap Shear (CRS St 1203); EN 1465
Dow BETAMATE™ 5103-2 Epoxy
BETAMATE™ 5103-2 is a one component heat curing Epoxy paste adhesive. The material is readily pumped at ambient temperatures. It shows excellent adhesion to automotive steel, including coated ste..