Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 15.0 MPa @Thickness 0.750 mm |
2180 psi @Thickness 0.0295 in |
Lap Shear (CRS St 1203); EN 1465 |
Dow BETAMATE™ 5103-2 Epoxy BETAMATE™ 5103-2 is a one component heat curing Epoxy paste adhesive. The material is readily pumped at ambient temperatures. It shows excellent adhesion to automotive steel, including coated ste.. |